Material Notes

Screen Mesh, Blade Type and Rotor Speed: What Actually Changes Regrind Quality

Three settings decide whether regrind feeds back cleanly or fills your parts with fines and dust. Here is what each one does, and which to change first.

Two granulators cutting the same runner can produce regrind that behaves completely differently in the press. The difference is not the motor. It is the screen, the cutting geometry and the rotor speed, in that order.

What good regrind looks like

Good regrind is uniform in size, low in dust, and free of long tails or flat plates that bridge in the feed throat. If you can pick up a handful and see three clearly different size classes, the granulator is not doing its job, and the press will show it as inconsistent shot weight or short shots.

Screen hole size: the first lever

The screen is the sizing gate. Material stays in the chamber until it is small enough to pass, so the hole size sets both the output size and how long the material is beaten around.
  • Smaller holes: finer, more uniform regrind, more fines, more heat, lower throughput
  • Larger holes: faster throughput, coarser regrind, fewer fines, better for thick sections
Fines are the expensive part. They bridge in hoppers, they carry dust into the feed zone, and they melt at a different rate than the granulate. If you are fighting short shots after adding regrind, try a larger screen before you change anything else.

Rotor knives versus claw blades

A rotor with sharp, adjustable knives against a fixed bed knife shears material cleanly. Claw or hooked geometry grabs and tears, which is more forgiving on bulky purgings and thick sections but produces more irregular particles.
For runners and rejects from a normal molding cell, sharp shear geometry with a properly gapped bed knife gives the most consistent result. Check the gap: a worn bed knife gap is the most common cause of tails and dust, and it is a ten-minute adjustment that people put off for months.

Rotor speed and heat

Higher rotor speed cuts faster and throws material out harder, but it also puts more energy into the plastic. Heat matters differently by material:
  • PP and PE tolerate heat well; slight softening is not a problem
  • ABS and PS mark and smear if the regrind gets warm
  • PA and PC pick up moisture and can degrade; warm regrind plus humid air is a bad combination
  • PVC is the sensitive one: heat history and dust are both problems, and regrind should be kept coarse and cool
If the granulate comes out warm to the touch, the machine is doing more work than it needs to. A larger screen and a lower rotor speed usually fix it.

When regrind needs blending or drying

Regrind is not the same material as virgin granulate. It has a different bulk density, a different particle shape, and often a different moisture level after sitting in a bin. Two practical rules:
  • Blend by weight, not by volume, if you are metering regrind back in
  • Dry hygroscopic regrind the same way you dry virgin material, and do not assume the dryer settings carry over

What to change first

When regrind quality is the problem, work in this order: bed knife gap, screen size, rotor speed, blade geometry. The first two cost almost nothing and fix most cases. Replacing a rotor is the last resort, not the first move.
See the granulator range, or read how to size a granulator before you change the machine.