Buying Guides
Closed-Loop Recycling: When Regrind Can Go Straight Back Into the Machine
Running regrind back into the same press is the cheapest material saving in a molding cell, and the fastest way to lose a customer if it is done without a trial procedure.
Closed-loop recycling means the sprue or reject leaves the mold, gets ground at the press, and goes back into the same machine without leaving the cell. It saves material and handling, and it can quietly change the parts you ship.
What closed-loop actually requires
Four things have to be true before regrind goes back in:
- The material is identified and consistent, not a mix of unknown resins
- The granulator produces uniform regrind with low dust
- Contamination is controlled: no metal, no cardboard, no purge block fragments
- Someone has agreed the regrind ratio with the customer, in writing
The fourth one is where projects fail. A molder starts at 20 percent, the parts pass, and nobody records it. Two years later a new customer asks for virgin-only material and the process has no documented history.
Regrind ratio: start low and document it
There is no universal ratio, because the limit depends on wall thickness, gate design, material and the end use. What matters is that the ratio is chosen deliberately and recorded.
A practical approach for a first trial:
- Start at 10 percent regrind by weight
- Run a full shift on a stable mold, not on the hardest job in the plant
- Check dimensions, weight, color and any mechanical requirement the part has
- Increase in 5 percent steps, with the same checks each time
- Stop at the first sign of short shots, weld line movement or color drift
Thin walls, long flow paths and glass-filled materials are the cases where the limit arrives early. Thick sections and non-critical parts tolerate more. Write the number you settled on into the setup sheet, not into someone's memory.
Contamination control is the real work
The granulator does not know what it is cutting. Three cheap controls cover most risk:
- A metal detector or magnet before the feed opening
- Clear instructions on what never goes in: purge blocks from other materials, printed film, cardboard, floor sweepings
- A dedicated bin per material, labelled, with the lid on
If the cell changes materials frequently, a colour change is the moment regrind gets mixed. Flush the granulator and the bin, or accept that the first hour of regrind is scrap.
Feeding regrind back in
Two common ways, with different consequences:
- A proportioning valve on the machine throat: cheap, simple, but the ratio drifts when granulate bulk density changes
- A gravimetric blender: costs more, holds the ratio by weight, and gives you a record you can show a customer
For a single machine running one material, the valve is usually enough. For anything customer-audited, the blender pays for itself in documentation alone.
Safety and housekeeping
A granulator at the press introduces three hazards that a central system hides: rotating blades within reach of the operator, noise, and dust. Confirm that the feed hopper cannot be opened while the rotor turns, that the machine is on the correct interlock circuit, and that hearing protection is part of the cell, not an afterthought.
A trial procedure that survives an audit
- Record the material, batch and virgin/regrind ratio
- Record granulator settings: screen, rotor speed, blade condition
- Produce a first-article sample at the chosen ratio and keep it
- Log dimensions and weight for the first 50 shots
- Review after one shift, then after one week
- Write the approved ratio into the setup sheet and the customer file
That is a day of work that turns a cost saving into a process you can defend.
Start with the granulator range, or send your material and reject rate through the contact form for a sizing check.